Paint peeling off new plaster?

0:07 videoPosted 21 November 2026

This short video explains why paint peels off new plaster, and why a missing mist coat is usually the cause. Fresh plaster is very thirsty. When full-strength paint is rolled straight onto it, the plaster sucks the water out of the paint before it can grip, so the paint dries as a skin on the surface. A few weeks or months later it starts to crack, lift and flake off in patches.

The proper way to paint bare plaster is with a mist coat, a watered-down first coat that soaks into the plaster and gives the top coats something solid to grip. The video uses Graphenstone Naturcolor, a breathable mineral emulsion that works as its own primer, under eco paints such as Graphenstone GrafClean, GCS and Siena.

Let new plaster dry fully first, for at least 28 days, until it is an even, pale colour. Thin the Naturcolor with 10 to 15% water and apply one coat. If paint is already peeling, scrape off everything loose, sand the edges smooth, then mist coat the bare patches and repaint.

See the original on Instagram
Transcript

Paint peeling off new plaster?

Bare plaster is thirsty. It sucks the water out of paint before it can grip.

So the paint dries as a skin on top, then cracks and peels off later.

The proper way is a mist coat: the bridge between thirsty plaster and your paint.

We use water-thinned Graphenstone Naturcolor. Already peeling? Scrape back first.

Products we recommend

Questions about this video

Ask a question about this video

We reply by email, and we may add your question and our answer to this page (without your name).

More videos like this

See all our videos